J Dent Sch GYEAR__, 22(4): 557-566 Back to browse issues page
Effect of HEMA on shear bond strength of enamel bonding to dentin after 1 year
Roya Aminian DCorresponding Author: r. *1, Golrokh Saeedi Dr.
Abstract:   (5899 Views)

Purpose: Adhesion to dentin is the major problem in using tooth color composite resins. The way proposed is the use of hydrophile resins, of which, HEMA is the most important one. Because of the importance of the subject, this study was conducted to evaluate the effect of HEMA on shear bond strength of enamel bonding agent to dentin after 1 year water storage.

Methods & Materials: This invitro study carried out experimentally on 36 extracted premolar teeth. The teeth randomly assigned to 4 groups, each group containing 6 samples. In group 1, the solution of %35 HEMA and Acetone and in group 2, the solution of %35 HEMA and Water was used. Multipurpose Scotchbond primer was used in group 4. In group 1 and 2, enamel bonding and in group 4 the adhesive was used. In group 3, teeth were dried and enamel bonded after etching. Composite cylinders were bonded on the areas with the same dimensions. The prepared samples were thermocycled 1000 times at 55°C and 5°C after keeping in distilled water for 1 year. Shear bond strength of the samples were tested by Instron machine.

Results: Results showed that the "HEMA and Acetone" group had the highest strength (25.12±3.52), and then, "Scotchbond" group (23.55±1.6). "HEMA and Water" group (14.31±5.6) and "enamel bonding" group (4.25±2.61) had the next ranks respectively. Analysis of variance test showed that the overall difference between them was statistically significant (P<0.0001). Difference in strength of HEMA and Scotchbond was not significant but was significantly different from other groups.

Conclusion: Shear bond strength of "HEMA and Acetone" and "HEMA and Scotchbond" became acceptable after thermocycling and storage in distilled water for one year but not in enamel bonding group.

J Dent Sch 2005 22(4): 557

Keywords: HEMA, Shear Bonding Strength, Dentin, invitro
Full-Text [PDF 158 kb]   (1377 Downloads)    
Type of Study: Original Article | Subject: Special
Received: 2006/09/6
Add your comments about this article
Your username or Email:

CAPTCHA


XML     Print


Download citation:
BibTeX | RIS | EndNote | Medlars | ProCite | Reference Manager | RefWorks
Send citation to:

Aminian R, Saeedi G. Effect of HEMA on shear bond strength of enamel bonding to dentin after 1 year . J Dent Sch. 2005; 22 (4) :557-566
URL: http://jds.sbmu.ac.ir/article-1-378-en.html


Volume 22, Issue 4 (Winter 2005) Back to browse issues page
مجله دانشکده دندانپزشکی دانشگاه علوم پزشکی شهید بهشتی Shahid Beheshti University Dental Journal
Persian site map - English site map - Created in 0.05 seconds with 32 queries by YEKTAWEB 3961