Comparing the Effect of Topical Acidulated Phosphate Fluoride on Micro-Hardness of Two Fissure Sealants and One Flowable Composite
R Mazaheri, L Pishevar *, N Keyhanifard, E Ghasemi
Assistant Professor Dept. of Operative Dentistry , l.pishevar@khuisf.ac.ir
Abstract:   (2295 Views)

  Objective: Probable effect of fluoride containing materials like APF on sealants is very important. The purpose of this study is to assess the effect of frequent application of APF (1.23%) on the surface microhardness of two fissure sealants and one flowable composite.

  Methods: In this experimental study, 81 specimens of two fissure sealants and one flowable composite were prepared, using special polymer mold in three groups of 27 including unfilled resin sealant (Fissurite F, Voco), filled resin sealant (Fissurit FX, Voco) and one flowable composite (Arabesk Flow, Voco). Then, these three groups were divided into three sub groups of 9 as follows: Group 1, 4, 7 (control): No treatment- Group 2, 8, 5: Single application using APF- Group 3, 6, 9: Six times application using APF. The APF was applied on the experimental specimens every time for 4 minutes. Then, the samples were stored in the distilled water. Finally, the surface microhardness of the sealants was measured using Vickers test. The statistical analysis was performed by 2-way ANOVA & One-way ANOVA tests.

  Results: Type of materials (without filler, containing filler and flowable composite) was effective on the surface microhardness and the difference between three types of materials was statically significant (p<0.001).Unfilled fissure sealants, showed minimum surface microhardness and flow able composite showed maximum surface microhardness. Also, the frequency of gel use (once or many times), had no effect on the average surface microhardness of the materials under review (p>0.05).

Conclusion: All three materials were resistant to the destructive effects of APF gel and it did not make a significant microhardness changes
Keywords: Acidulated phosphated fluoride, Dental caries, Fissure sealants, Flowable camposite, Surface microhardness, Prevention
Full-Text [PDF 123 kb]   (678 Downloads)    
Type of Study: Original Article | Subject: Special
Received: 2014/04/22 | Accepted: 2014/04/22 | Published: 2014/04/22
Send email to the article author

Add your comments about this article
Your username or email:

Write the security code in the box >



XML     Print


Download citation:
BibTeX | RIS | EndNote | Medlars | ProCite | Reference Manager | RefWorks
Send citation to:

Mazaheri R, Pishevar L, Keyhanifard N, Ghasemi E. Comparing the Effect of Topical Acidulated Phosphate Fluoride on Micro-Hardness of Two Fissure Sealants and One Flowable Composite. J Dent Sch. 2014; 32 (2) :103-110
URL: http://jds.sbmu.ac.ir/article-1-1243-en.html
Volume 32, Number 2 (Spring 2014) Back to browse issues page
مجله دانشکده دندانپزشکی دانشگاه علوم پزشکی شهید بهشتی Shahid Beheshti University Dental Journal
Persian site map - English site map - Created in 0.05 seconds with 792 queries by yektaweb 3463